TITLE

Analytical model for island growth in atomic layer deposition using geometrical principles

AUTHOR(S)
Nilsen, O.; Mohn, C. E.; Kjekshus, A.; Fjellvåg, H.
PUB. DATE
July 2007
SOURCE
Journal of Applied Physics;7/15/2007, Vol. 102 Issue 2, p024906
SOURCE TYPE
Academic Journal
DOC. TYPE
Article
ABSTRACT
Island growth has been shown to also occur for atomic layer deposition (ALD) processes. This article presents a relatively simple analytical model using geometrical principles with few independent variables on evolution of thickness and roughness in island-dominated ALD processes. The model is well suited for the fitting of experimental data to extract parameters such as density of islands and growth rate. It allows islands of various shapes, but most of the attention here is devoted to cone and hemispherical shaped islands in a hexagonal grid on a flat substrate. For a selection of cases, exact analytical expressions are derived. The model shows that it is possible to reproduce the growth characteristics of substrate-inhibited growth of both types 1 and 2 with a suitable choice of functional form of the islands. Finally it is compared with previously advanced models describing substrate-inhibited growth.
ACCESSION #
26017543

 

Related Articles

  • Why Philosophical History is Essential to Teaching the Second Law of Thermodynamics. Trout, Bernhardt L. // AIP Conference Proceedings;8/12/2008, Vol. 1033 Issue 1, p288 

    This proceeding discusses the motivation for and nature of a new course developed at MIT by the author and Dr. Lee Perlman. The course, entitled “A Philosophical History of Energy” (10.04/24.114), teaches students about the fundamental issues behind scientific theories of energy with...

  • phys·ics.  // American Heritage Student Science Dictionary;2009, p266 

    The article presents an encyclopedia definition for the term "physics," which refers to the scientific study of matter and energy and the relations between them.

  • Insignificance. Carroll, Sean // Nature;5/6/2004, Vol. 429 Issue 6987, p27 

    Explores the introduction of the concept of dark matter and dark energy. Discovery of the concept in 1933 by Fritz Zwicky; Independent ways to measure the amount of ordinary matter; Inference on the existence of dark matter and dark energy indirectly.

  • THE MULTISCALE MODEL COMBINING ELASTIC THEORY WITH AB INITIO CALCULATIONS FOR METAL–CERAMIC INTERFACES. ZHANG, YING; YAO, YUGUI // Modern Physics Letters B;12/30/2008, Vol. 22 Issue 32, p3135 

    The generalized two-dimensional Peierls–Nabarro (PN) model7 for studying interfaces is developed further, where an exact generalized stacking fault energy γ-surface obtained from ab initio calculations acts as an input function for the generalized PN model. Using the multiscale...

  • Paranormal Phenomena, Physics and Dirac Energy. Borutta, Rich // Journal of Spirituality & Paranormal Studies;Oct2009, Vol. 32 Issue 4, p192 

    Experiments in low temperature physics have indicated the possibility of an extreme state of matter and energy characterized by negative energy that was predicted in 1928 by P. A. M. Dirac. A modern interpretation of that concept by D. L. Hotson describes a domain of negative energy,...

  • What is energy?  // Monkeyshines on America;Nov99 Alternative Energy Sources, p2 

    Discusses facts about energy. Definition of terms; Unit of measurement.

  • How do we use energy?  // Monkeyshines on America;Nov99 Alternative Energy Sources, p3 

    Discusses various ways of using energy. Living and non-livign things that use energy; Conservation of energy.

  • History of Energy.  // Monkeyshines on America;Nov99 Alternative Energy Sources, p8 

    Discusses the history of energy. Discovery of fire; Tools to harness the energy of animals; Use of pulleys and levers; Sources fo alternative energy.

  • What Is Force? Dalton, Cindy Devine; Sikora, Teresa; Sikora, Ed // Force & Motion;2001, p8 

    The article describes force. The more mass an object has, the more force it takes to move it. The faster an object moves, the more force required to stop it.

Share

Read the Article

Courtesy of THE LIBRARY OF VIRGINIA

Sorry, but this item is not currently available from your library.

Try another library?
Sign out of this library

Other Topics